MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

USI Corporation EVATHENE® UE630 EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Description: EVATHENE® UE630 is an ethylene-vinyl acetate copolymer resin (EVA) for use in foam injection, foam compression molding, sheet extrusion, blown molding, casting and co-extrusion machine.

Characteristics:

  • Flexibility
  • Elasticity
  • Great resistance to environmental stress cracking
  • Low temperature flexibility
Main Application:
  • Shoe sole foaming
  • Food packaging

Information provided by USI Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ASTM D792
Vinyl Acetate Content 16 %16 %USI
Melt Flow 1.5 g/10 min1.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ASTM D2240
Tensile Strength at Break 16.7 MPa2420 psiMolded; ASTM D638
Elongation, Ultimate 700 %700 %Molded; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 89.0 °C192 °FASTM D3418
Vicat Softening Point 67.0 °C153 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUSIC009 / 285377

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.