MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt Gravicol 2428 TC Bonding Paste-Fiber
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Pre-accelerated bonding paste based on unsaturated polyester resin. Cures at room temperature (15 - 25°C). Cured using MEKP peroxide.

Appearance: TC : Contains catalyst indicator

Use Areas: Product suitable for many types of thick joint bonding of composite parts. The product meets requirements for the operations of gap filling, surface filling and sealing. The product can be used as a laminating aid.

Application: Surface to be bonded should be free from dust and contaminants which can adversely affect the bond adhesion strength. Preparation of surface is recommended using light abrasion / sanding followed by cleaning with appropriate solvent. The bonding paste is ready to use and reaction is initiated using the correct dosage of correct peroxide. Typical dosage is 1% to 2% w/w under normal workshop application conditions (15-25°C). Mix thoroughly to ensure homogeneous catalyst dispersion (this is assisted by use of catalyst indicators which change color in TC version). Apply a uniform bead of bonding paste onto one of the surfaces and press parts together evenly to obtain the desired thickness of bond. Typically the thickness of the joint is greater than 5mm. Allow sufficient time for cohesive bond to form between laminates before handling bonded parts.

Properties / Advantages: Semi flexible bonding paste for dynamic bonding applications. Bonding paste with fibers for thick joints. Very smooth consistency, and easy to apply with a spatula or comb applicator. Due to its non shrinkage characteristics, dimensional stability of part is maintained during the curing cycle of the paste. Not suitable for use in thick bond applications.

Storage / Shelf Life: Shelf-life : 6 Months. When the product is sealed in its original packing, stored indoors away from direct sunlight and direct heat sources and ideally at ambient temperature between 15°C and 25°C .

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 - 1.35 g/cc0.0462 - 0.0488 lb/in³
Viscosity 4000 - 6000 cP4000 - 6000 cPSpindle V73 - 0.5 rpm
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 29.0 MPa4210 psiNFP 15-451
Compressive Strength 57.5 MPa8340 psiNFP 15-451
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 75.0 min
@Temperature 23.0 °C
0.750 - 1.25 hour
@Temperature 73.4 °F
Peak; Catalyst : MEKP - (250g - 1% MEKP); MT-C B 072 R
Gel Time 15.0 - 23.0 min
@Temperature 23.0 °C
15.0 - 23.0 min
@Temperature 73.4 °F
Catalyst : MEKP - (250g - 23°C - 1% MEKP)
Shelf Life 6.00 Month
@Temperature 15.0 - 25.0 °C
6.00 Month
@Temperature 59.0 - 77.0 °F
 
Descriptive Properties
Bond failure in the laminate4 hrMT-C B 901 Q
Peak Exotherm100-120°CMT-C B 072 R; Catalyst : MEKP - (250g - 23°C - 1% MEKP)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9001 / 231596

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.