MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

HB Fuller 1535 Silicone adhesive sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 1535 is one-component, silicone adhesive sealant that cures on exposure to atmospheric moisture to form an silicone elastomer. This material offers excellent electrical properties, weather stability, chemical resistance, flame retardancy and thermal conductivity.

Features and Benefits:

  • Good adhesion to most common building substrates, like glass, metal, plastics, FR4, lead frames, etc.
  • High thermal conductivity
  • Excellent flexibility
  • Low odor
  • Neutral, non-corrosive
  • Flame retardant
Typical Applications:
  • Thermal interface material
  • Thermal conductive encapsulation
  • Protects leads from mechanical shock
  • Electronics encapsulation
  • Sealing and waterproofing

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.60 g/cc2.60 g/cc
Storage Temperature 5.00 - 25.0 °C41.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282GB/T531
Tensile Strength 3.50 MPa508 psiGB/528
Elongation at Break 180 %180 %GB/528
Shear Strength 1.50 MPa218 psiLap Joint, Aluminum; GB/T7124
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 210 °C410 °F
Minimum Service Temperature, Air -54.0 °C-65.2 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 3.00 min0.0500 hourTack Free Time
 1440 min
@Thickness >=2.00 mm
24.0 hour
@Thickness >=0.0787 in
Full Cure
 
Descriptive Properties
ColorWhite
ConsistencyThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL108 / 316899

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.