MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastics Group Polifil® GFPPCC-3005WS 30% Glass Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Polifil® GFPPCC-WS series compounds are Water Safe Homopolymer polypropylenes reinforced with chemically coupled glass fibers and are certified to NSF/ANSI/CAN 61 Standard, and meet the regulatory requirements of the U.S. and Canada for Drinking Water System Components. These compounds offer superior strength and stiffness, improved elevated temperature performance, better creep resistance, higher impact strength and higher resistance to high temperature water than conventional glass fiber reinforced polypropylenes. Polifil® GFPPCC products are UL94 HB rated. These compounds are used in chemical resistance applications, appliances, electrical components, automotive, irrigation, utility, filter systems, and potable water products. Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Filler Content 30.0 %30.0 %TPG WI
Water Absorption 0.0300 %
@Time 86400 sec
0.0300 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.00400 cm/cm
@Thickness 2.49 mm
0.00400 in/in
@Thickness 0.0980 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.00900 cm/cm
@Thickness 2.49 mm
0.00900 in/in
@Thickness 0.0980 in
ASTM D955
Melt Flow 5.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psiASTM D638
Elongation at Break 4.50 %4.50 %ASTM D638
Flexural Yield Strength 106 MPa15400 psiASTM D790
Flexural Modulus 5.45 GPa790 ksitangent; ASTM D790
Izod Impact, Notched 0.854 J/cm1.60 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 154 °C310 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C290 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 221 °C410 - 430 °F
Middle Barrel Temperature 216 - 227 °C420 - 440 °F
Front Barrel Temperature 227 - 238 °C440 - 460 °F
Nozzle Temperature 227 - 249 °C440 - 480 °F
Melt Temperature 232 - 260 °C450 - 500 °F
Mold Temperature 48.9 - 65.6 °C120 - 150 °F
Drying Temperature 180 - 220 °C
@Time 3600 - 7200 sec
356 - 428 °F
@Time 1.00 - 2.00 hour
Back Pressure 0.172 - 0.517 MPa25.0 - 75.0 psi
Screw Speed 30.0 - 60.0 rpm30.0 - 60.0 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLI102 / 325315

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.