This gas phase, high molecular weight, ethylene-hexene copolymer with antistatic agent is tailored for lightweight blow molded parts that require: Excellent stiffness to ESCR ratio; Good impact resistance; Durability; Recyclability. Typical blow molded applications for 9513H include: Household and industrial chemical containers; Personal care product containers. information provided by Chevron Phillips Chemical Company LP. |