MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F515 Epoxy Resin, T2C120 Carbon Tape
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Hexcel designation: TXX120-12"-F515; Fiber: Toho® G30/500

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  1931 MPa
@Temperature 23.0 °C
280100 psi
@Temperature 73.4 °F
 1937 MPa
@Temperature 71.0 °C
280900 psi
@Temperature 160 °F
1/2 hr
Tensile Modulus  103.4 GPa
@Temperature 23.0 °C
15000 ksi
@Temperature 73.4 °F
 110.3 GPa
@Temperature 71.0 °C
16000 ksi
@Temperature 160 °F
1/2 hr
Flexural Yield Strength  1338 MPa
@Temperature 71.0 °C
194100 psi
@Temperature 160 °F
1/2 hr
 1351 MPa
@Temperature 23.0 °C
195900 psi
@Temperature 73.4 °F
Flexural Modulus  108.3 GPa
@Temperature 23.0 °C
15710 ksi
@Temperature 73.4 °F
 117.2 GPa
@Temperature 71.0 °C
17000 ksi
@Temperature 160 °F
1/2 hr
Compressive Yield Strength  1076 MPa
@Temperature 71.0 °C
156100 psi
@Temperature 160 °F
1/2 hr
 1158 MPa
@Temperature 23.0 °C
168000 psi
@Temperature 73.4 °F
Compressive Modulus  93.1 GPa
@Temperature 71.0 °C
13500 ksi
@Temperature 160 °F
1/2 hr
 106.9 GPa
@Temperature 23.0 °C
15500 ksi
@Temperature 73.4 °F
Shear Strength  75.8 MPa
@Temperature 71.0 °C
11000 psi
@Temperature 160 °F
Short Beam, 1/2 hr
 92.4 MPa
@Temperature 23.0 °C
13400 psi
@Temperature 73.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite
Hexcel® HexMC® C / 2000 / R1 Composite SMC
Hexcel® Fibrelam® 2000 Grade 5 Panels for Aircraft Flooring
Hexcel® Fibrelam® 2000 Grade 1 Panels for Aircraft Flooring
Goodfellow Carbon-Carbon Composite

PHEXC127 / 98597

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.