MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTOSINT® 1174 white Polyamide 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTOSINT 1164 white respectively 1174 white are nylon 12 fine powders which are specially developed for the minicoat process of small articles, e.g. corsetry or ferrit rings. VESTOSINT 1164 white and 1174 white are used additionally in paints.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
Water Absorption 1.65 %
@Temperature 100 °C
Immersion; ISO 62
Moisture Absorption 0.500 %50% RH; ISO 62
 1.20 %96% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ISO 868
Ball Indentation Hardness 101 MPaH30; ISO 2039-1
Taber Abrasion, mg/1000 Cycles <= 1.0CSI 7, 500g; ASTM D 1242
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Dielectric Strength 85.0 kV/mmIEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 104 µin/in-°F
@Temperature 23.0 - 55.0 °C
ISO 11359
Specific Heat Capacity 2.27 J/g-°CDIN 53765
Thermal Conductivity 0.220 - 0.270 W/m-KDIN 52612
Melting Point 176 °CISO 3146
 
Descriptive Properties
Active matterK20/P50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTOSINT® 1101 white Polyamide 12
Evonik VESTOSINT® 1161 white Polyamide 12
Evonik VESTOSINT® 1184 white Polyamide 12
Evonik VESTOSINT® 1164 white Polyamide 12
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing

PEVONIL178 / 196382

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.