MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Monprene® CP-17250 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-17200 Filled, High Flow Series of thermoplastic elastomer compounds, with good UV resistance, available in NAT or colors, from 40 to 80 Shore A, are designed specifically for EU consumer product applications requiring a soft, rubber-like feel. Monprene CP-17250 is a low hardness, high density grade that is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion; Good Colorability; Good Flexibility; Good Flow; Good Moldability; High Density; High Specific Gravity; Low Hardness; Lubricated; UV Resistant

Uses: Bushings; Consumer Applications; Flexible Grips; Gaskets; Grommets; Handles; Luggage; Overmolding; Plugs; Rubber Replacement; Soft Touch Applications

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Viscosity 109 cP
@Shear Rate 206 1/s,
Temperature 200 °C
109 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 50
@Time 5.00 sec
50
@Time 0.00139 hour
ISO 868
Tensile Strength at Break 7.93 MPa1150 psiISO 37
Tensile Stress at Strain  1.30 MPa
@Strain 100 %
189 psi
@Strain 100 %
ISO 37
 1.90 MPa
@Strain 300 %
276 psi
@Strain 300 %
ISO 37
Elongation at Break 900 %900 %ISO 37
Compression Set  22 %
@Temperature 22.8 °C,
Time 79200 sec
22 %
@Temperature 73.0 °F,
Time 22.0 hour
Method B; ISO 815
 43 %
@Temperature 70.0 °C,
Time 79200 sec
43 %
@Temperature 158 °F,
Time 22.0 hour
Method B; ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 120 - 160 °C248 - 320 °F
Middle Barrel Temperature 160 - 230 °C320 - 446 °F
Front Barrel Temperature 180 - 230 °C356 - 446 °F
Nozzle Temperature 180 - 230 °C356 - 446 °F
Melt Temperature 180 - 230 °C356 - 446 °F
Mold Temperature 15.0 - 50.0 °C59.0 - 122 °F
Back Pressure 0.500 - 1.50 MPa72.5 - 218 psi
Cushion 0.300 - 2.00 cm0.118 - 0.787 in
Screw Speed 30 - 100 rpm30 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0785 / 237276

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.