MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 3483-3 TFE 15  Liquid Crystal Polymer (LCP) Carbon Fiber 20% - PTFE 15%  (discontinued **)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Carbon Fiber Filled

Material Notes: Carbon Fiber 20% - PTFE 15%

Comments:

  • Carbon Fiber
  • PTFE Lubricated

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Filler Content 20 %
Linear Mold Shrinkage 0.00050 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 18000 psiASTM D638
Elongation at Break 0.90 %ASTM D638
Modulus of Elasticity 3900 ksiASTM D638
Flexural Yield Strength 28000 psiASTM D790
Flexural Modulus 2900 ksiASTM D790
Izod Impact, Notched 0.900 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 7.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+8 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 550 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.59 mm
Per testing by RTP Company; ASTM D3801
 
Processing PropertiesOriginal ValueComments
Processing Temperature 635 - 670 °F
Mold Temperature 150 - 250 °F
Injection Pressure 12000 - 18000 psi
 
Descriptive Properties
ColorNatural/Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 3485-3 Liquid Crystal Polymer (LCP), Carbon Fiber
Celanese VECTRA® 2355MT Carbon Fiber Reinforced Liquid Crystal Polymer (LCP)
RTP Company RTP 3483-3 Liquid Crystal Polymer (LCP), Carbon Fiber
RTP Company RTP 3485-3 TFE 15  Liquid Crystal Polymer (LCP) Carbon Fiber 30% - PTFE 15%
RTP Company RTP 3485-4 Liquid Crystal Polymer (LCP), Carbon Fiber

PR5152 / 64505

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.