MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Syncure™ V0044G S-1 RoHS Natural Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.24 g/ccASTM D792
Density 1.26 g/ccGeon® 1169; Internal Method
Melt Flow 3.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Procedure A; ASTM D1238
 
Descriptive Properties
FeaturesFast Cure
 Flame Retardant
FormsPellets
Generic MaterialXLPE
Generic NamePolyethylene, Crosslinked (XLPE)
Regional AvailabilityNorth America
UsesWire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Syncure™ System S112NA Polyethylene, Crosslinked (XLPE)
Graft Polymer GRAFTABOND™ UH-SAN 00055 PDIM Ultra High Molecular Weight Polyethylene, grafted with Styrene Acrylonitrile
Borealis Visico™/Visico™ LE4423/LE4438 Polyethylene Compound, Crosslinkable
Borealis LE4217 Polyethylene Compound, Crosslinkable, Track Resistant
Borealis Borlink™ LE4244S Polyethylene Insulation Compound, Crosslinkable

PH0POL1455 / 146024

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.