General core type with an intermediate particle size distribution for Equiax castings. Formulated to be used for large land-based type cores that require good stability at elevated temperatures and for chunky airfoil cores up to 30 inches long, 8 inches wide, and 1 inch thick.information provided by Morgan Advanced Materials |