MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECACOMP PBT GF30 natural 1014807 PBT, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes:

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/inDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inDIN EN ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 140 MPa20300 psiDIN EN ISO 527-1
Elongation at Break 3.5 %3.5 %DIN EN ISO 527-1
Modulus of Elasticity 9.20 GPa1330 ksiDIN EN ISO 527-1
Charpy Impact Unnotched 6.50 J/cm²30.9 ft-lb/in²DIN EN ISO 179-1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F
Maximum Service Temperature, Air 110 °C230 °Flong term
 170 °C338 °Fshort term
Glass Transition Temp, Tg 60.0 °C140 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 - 275 °C464 - 527 °FCylinder
Melt Temperature 260 - 280 °C500 - 536 °FMaterial temperature
Mold Temperature 60.0 - 130 °C140 - 266 °F
Drying Temperature <= 120 °C<= 248 °F
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hour
 
Descriptive Properties
Colornatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9038 / 318966

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.