Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensive machining. Typical applications include parts for printing and packaging machines, as well as conveying systemsInformation provided by manufacturer |