MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco CERAMACAST™ 578 High Moisture Resistant Silicone for Small Potting
Categories: Ceramic; Oxide; Silicon Oxide; Potting/Casting Ceramic

Material Notes: Aluminum oxide filled silicone adhesive. Aremco Ceramacast™ products provide the most expansive range of ceramic- and silicone-based materials for the assembly of high temperature, high power electrical devices, fixtures, molds and tooling.

Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 12.5 lb/gal10 lb/gal Powder; 2.5 lb/gal Liquid
Porosity <= 0.50 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cm
Dielectric Strength >= 250 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µin/in-°F
Maximum Service Temperature, Air 900 °F
Shrinkage <= 1.0 %
@Temperature 538 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 hour
Shelf Life 12.0 Month
 
Descriptive Properties
Acid ResistanceGood
Alkali ResistanceGood
ColorWhite
Mix Ratio100:20-25
Moisture ResistanceExcellent
ViscosityPasteMixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CAREM955 / 316314

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.