MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess LEWATIT® K 6367 Copolymer Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® K 6367 is a strongly basic (type I), gel-type resin based on a copolymer of styrene and divinylbezene. By the presence of large beads, connected with a monodisperse particle size distribution of the beads, the flow through the resin bed happens homogeneously and with a comparatively low pressure loss. At the same time, the risk of accumulation of suspended solid particles is significantly lower than in the case of ion-exchange resins with a “standard distribution of bead size’. Reaction parameters can be maintained in even tighter tolerances, if the catalyst is used in flow processes. The Lewatit K 6367 is particularly suitable for:
  • The recovery of uranium form alkaline and acidic process streams
  • The removal and recovery of heavy metal anionic complexes such as the chloride and cyanide solutions.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.755 g/cc0.0273 lb/in³
Density 1.08 g/cc0.0390 lb/in³
Bead Size 0.750 - 0.850 mm0.0295 - 0.0335 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceLight yellow, translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8763 / 209155

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.