MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex UNIPRENE® 7400-64 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes:

Information provided by Teknor Apex Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 64645 seconds; ASTM D2240
Tensile Strength, Yield 2.76 MPa400 psiAdhesion to EPDM, 0.125" Micro Die, 8"/min; ASTM D412
 4.69 MPa680 psi85% Retention, Hot Air Aging, 22 hrs at 70°C
 5.52 MPa800 psiASTM D412
Elongation at Break 320 %320 %80% Retention; Hot Air Aging, 22 hrs at 70°C
 400 %400 %ASTM D412
Elongation at Yield 100 %100 %Adhesion to EPDM, 0.125" Micro Die, 8"/min; ASTM D412
100% Modulus 2.76 MPa
@Strain 100 %
400 psi
@Strain 100 %
ASTM D412
Compression Set  29 %
@Temperature 23.0 °C,
Time 79200 sec
29 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395, Method B
 42 %
@Temperature 70.0 °C,
Time 79200 sec
42 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395, Method B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Termopol Termoton® V2GA0065A TPV Compound
Termopol Termoton® V2GA1065A TPV Compound
Termopol Termoton® V6GA3075A TPV Compound
Stellarchem SV-B65E TPV Compound

PTEKNO244 / 69987

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.