MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Resin Technology Group MX-2212 High Impact, Multi-Functional, UV Curing Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: This multi-functional product is a rapid setting structural adhesive. UV-MX 2212 provides high impact, resilient bonds to many similar and dissimilar substrates. Multi-functional cure bonds are formed very rapidly by using activator, heat or exposure to ultraviolet light. UV-MX 2212 is a general purpose structural, multi-functional UV curing system designed for bonding, potting and sealing applications. Bonds exhibit both toughness and flexibility and perform well under stress caused by different coefficients of expansion. UV cured bonds are translucent to 1/4” thick sections, the maximum suggested UV curable bondline thickness.

Applications:

Metal bonding, fillet/sealing or bridging. Encapsulation/ unitizing potting laminations. Typical uses: DC motor construction, Magnet bonding, Pump motor housings, Audio speakers, Pot cure bonding, Mounting plates.

Processing:

Activator Cure: Bondline thickness of 0.02"; Fixture time of 20-30 seconds; 95% full strength in 1 hour; Full cure in 18 hours.

Thermal Cure: Heat can be used as a secondary cure mechanism only after UV light curing for surfaces exposed to air. 1 hour at 225°F; 1/2 hour at 250°F; 15 minutes at 300°F.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 1.2 %Cured
Viscosity 5000 cP
@Temperature 25.0 °C
Standard, uncured
 25000 cP
@Temperature 25.0 °C
T-grade, uncured
Thickness <= 5080 micronsCured film, activator cure
 <= 6350 micronsCured film, UV cure
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40 - 50Cured
Tensile Strength at Break 2500 psiCured
Elongation at Break 160 %Cured
Shear Strength 2500 psiCured, lap, steel/steel
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 480 V/milCured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °CCured
Minimum Service Temperature, Air -45.0 °CCured
Flash Point >= 200 °FUncured
Shrinkage 7.0 %Upon Cure
 
Descriptive Properties
ColorLight Straw
CompositionUrethane Oligomer/ (Meth) Acrylate Monomer Blend
SolubilityIsopropyl Alcohol, Chlorinated solvents
ViscosityThixo PasteGel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Imidex Thermoplastic Polyimide
Sandvik Kanthal PAC-240 Wire insulations and coatings
Master Bond FLM36-LO Film Adhesive
Hexcel® Redux® 322 Modified epoxy film adhesive (0.078 psf)
Hexcel® Redux® 322 Modified epoxy film adhesive (0.05 psf)

PRESINT649 / 65533

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.