MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.08 - 1.62 g/ccAverage value: 1.50 g/cc Grade Count:28
Filler Content 10.0 - 40.0 %Average value: 32.1 % Grade Count:7
Water Absorption 0.0100 - 0.0300 %Average value: 0.0209 % Grade Count:10
Moisture Absorption at Equilibrium 0.0300 - 0.100 %Average value: 0.0575 % Grade Count:4
Linear Mold Shrinkage 0.000100 - 0.00500 cm/cmAverage value: 0.00167 cm/cm Grade Count:23
Linear Mold Shrinkage, Transverse 0.00250 - 0.0110 cm/cmAverage value: 0.00581 cm/cm Grade Count:8
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 53.0 - 180 MPaAverage value: 135 MPa Grade Count:28
Tensile Strength, Yield 53.0 - 177 MPaAverage value: 132 MPa Grade Count:3
Elongation at Break 0.000 - 2.00 %Average value: 1.19 % Grade Count:28
Modulus of Elasticity 4.60 - 34.5 GPaAverage value: 19.7 GPa Grade Count:22
Flexural Yield Strength 91.0 - 270 MPaAverage value: 204 MPa Grade Count:23
Flexural Modulus 9.00 - 27.6 GPaAverage value: 17.9 GPa Grade Count:23
Flexural Strain at Break 1.20 - 1.60 %Average value: 1.40 % Grade Count:4
Izod Impact, Notched 0.374 - 0.641 J/cmAverage value: 0.490 J/cm Grade Count:16
Izod Impact, Unnotched 2.14 - 4.43 J/cmAverage value: 3.05 J/cm Grade Count:12
Izod Impact, Notched (ISO) 5.70 - 8.00 kJ/m²Average value: 6.67 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 15.0 - 31.0 kJ/m²Average value: 23.7 kJ/m² Grade Count:5
Charpy Impact Unnotched 0.500 - 2.70 J/cm²Average value: 1.82 J/cm² Grade Count:11
Charpy Impact, Notched 0.380 - 0.650 J/cm²Average value: 0.458 J/cm² Grade Count:4
Falling Dart Impact 4.50 - 15.1 JAverage value: 8.17 J Grade Count:3
Instrumented Impact Total Energy 2.19 - 2.97 JAverage value: 2.53 J Grade Count:3
Coefficient of Friction 0.140 - 0.390Average value: 0.292 Grade Count:5
Coefficient of Friction, Static 0.180 - 0.340Average value: 0.280 Grade Count:5
K (wear) Factor 8.00 - 94.7 x 10-8 mm³/N-MAverage value: 36.0 x 10-8 mm³/N-M Grade Count:5
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00 - 1.00e+12 ohm-cmAverage value: 5.00e+10 ohm-cm Grade Count:14
Surface Resistance 25.0 - 1.00e+6 ohmAverage value: 72500 ohm Grade Count:8
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 - 60.0 µm/m-°CAverage value: 30.8 µm/m-°C Grade Count:5
Melting Point 278 - 281 °CAverage value: 280 °C Grade Count:7
Maximum Service Temperature, Air 220 - 260 °CAverage value: 239 °C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 260 - 280 °CAverage value: 268 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 152 - 277 °CAverage value: 256 °C Grade Count:26
Vicat Softening Point 240 - 255 °CAverage value: 250 °C Grade Count:3
Glass Transition Temp, Tg 90.0 - 94.0 °CAverage value: 91.0 °C Grade Count:4
Flammability, UL94 V-0Grade Count:11
 
Processing PropertiesOriginal ValueComments
Processing Temperature 288 - 370 °CAverage value: 311 °C Grade Count:9
Nozzle Temperature 320 - 340 °CAverage value: 330 °C Grade Count:3
Melt Temperature 290 - 370 °CAverage value: 321 °C Grade Count:16
Mold Temperature 120 - 200 °CAverage value: 152 °C Grade Count:24
Drying Temperature 50.0 - 150 °CAverage value: 127 °C Grade Count:17
Injection Pressure 30.0 - 103 MPaAverage value: 81.7 MPa Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler
Mitsubishi Chemical Advanced Materials Fluorosint™ 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler

O4528 / 78350

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.