MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polytek FormRub 35 Liquid Rubbers
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: FormRub Series Liquid Rubbers consist of two parts (A and B), which, after mixing, cure at room temperature to fl exible rubber. Molds made with FormRub are excellent for casting concrete, plaster and wax. In addition, when coated with a proper release agent, FormRub molds can be used to cast various resins and foams. FormRub Liquid Rubbers are formulated for good economy with high performance and durability.

Product Line Features:

  • Soft to firm, flexible mold rubbers
  • Low viscosity
  • Ideal for demanding, high-production casting and forming of concrete
  • Dimensionally stable and abrasion resistant – molds can last years
  • 1A:1B mix ratios

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Viscosity 600 cP600 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535
Tensile Strength 1.95 MPa283 psi
Elongation at Break 2250 %2250 %
Tear Strength 12.1 kN/m69.0 pliDie C Tear
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min0.250 hourPour Time
 960 min16.0 hourDemold Time
 
Descriptive Properties
Cured ColorTurquoise
Mix Ratio By Weight1A:1B
Specific Volume27.2 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTK5056 / 251048

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.