MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
C.O.I.M. LARIPUR® LPR70D60 PTMG Polyether Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:
  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Series 60 and E 2103 PTMG Ether: These products are based on PTMG polyether. In comparison to the LARIPUR® ester series, they show a higher resistance to hydrolysis and microbiological attacks, have higher cold flexibility but have lower thermal and oxidizing resistance.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72ASTM D2240
Tensile Strength, Yield 70.0 MPaASTM D412
Elongation at Break 310 %ASTM D412
50% Modulus 0.0303 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.0332 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0551 GPa
@Strain 300 %
ASTM D412
Flexural Modulus 0.950 GPaASTM D790
Izod Impact, Notched (ISO) 7.50 kJ/m²
@Temperature -20.0 °C
ASTM D256
Tear Strength 230 kN/mASTM D624
Abrasion 40mm3, Abrasion Loss; DIN 53516
Torsional Stiffness 232 MPa+20°C; ASTM D1043
 472 MPa-20°C; ASTM D1043
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 152 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR5260 PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR5760 PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR6260 PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR6560 PTMG Polyether Polyurethane

PCOIM033 / 28636

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.