MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Keltan® 7752C Ethylene-Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Amorphous, oil extended, ethylene-propylene rubber with high ENB (ethylidene norbornene) content and a high Mooney viscosity at 20 phr colorless oil extension. The Controlled Long Chain Branching technology of this grade combines excellent processing characteristics and physical properties. This combination makes the product highly suitable for sponge profiles requiring excellent surface quality and dimensional control. Main application areas for this grade is automotive sponge seals and waste water seals.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.870 g/cc
Mooney Viscosity 53
@Temperature 150 °C
(1+8); ISO 289
Storage Temperature >= 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.0 Month
 
Descriptive Properties
Content20 phrOil, ISO 1407
 45 percentEthylene, ASTM D3900
 7.5 percentENB, ASTM D6047

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess Keltan® 9950C Ethylene-Propylene Rubber
Lanxess Keltan® 5465Q Ethylene-Propylene Rubber
Lanxess Keltan® 5470Q Ethylene-Propylene Rubber
Lanxess Keltan® 6160D Ethylene-Propylene Rubber
Lanxess Keltan® 8550C Ethylene-Propylene Rubber

PLANY8595 / 208988

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.