MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ChevronTexaco Transultex® H
Categories: Fluid; Lubricant

Material Notes: Texaco Transultex metalworking fluids deliver value through:
  • Excellent antiweld properties from active sulfur and chlorine which reduce frictional heat, prevent welding of metal to the tool point, extend tool life and reduce power consumption in moderate to severe duty operations.
  • Transparent, light color allows operator to better see the machined part during the cutting operation.
  • Antimist control — Minimizes the amount of stray mist in the air around the machine and operator.

Texaco Transultex cutting oils are transparent, light color, low odor cutting oils containing chlorine and active sulfur. The product line varies in viscosity and EP level to cover the widest range of machining operations and conditions.

Texaco Transultex cutting oils contain effective antiweld additives that react at the chip-tool interface to form boundary lubricating films that reduce frictional heat and prevent welding of the tool and workpiece.

With the exception of Texaco Transultex D, the Texaco Transultex line of cutting oils contains fatty oil lubricity additives that provide better surface finish.

Texaco Transultex cutting oils are formulated with paraffinic base stocks with naturally high viscosity index. These cutting oils have high flash points, minimizing the potential for fire. They also contain an effective mist control agent that reduces stray mist around the machine. This improves shop cleanliness and reduces operator exposure to the cutting oil.

Texaco Transultex metalworking fluids:

  • Provide excellent cooling and lubrication in a wide
  • Range of machining operations
  • Prevent welding of chip and tool
  • Flush chips away from the work area
  • Protect the finished work surfaces, tools and machines against rusting and staining
  • Reduce oil mist in high-speed machine tools.

Texaco Transultex cutting oils vary in viscosity and compounding levels to cover a wide range of machining operations and conditions.

Texaco Transultex H has the highest level of EP compounding and is recommended for the most severe cutting operations on the most difficult metals and alloys.

Texaco Transultex cutting oils contain active sulfur that is staining to yellow metals. Texaco Transultex cutting oils should not be used to machine copper and its alloys.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221575; MSDS Number: 8906

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 24.5 °24.5 °
Saybolt Viscosity at 100°F 269 SUS269 SUS
Saybolt Viscosity at 210°F 52 SUS52 SUS
Kinematic Viscosity at 40°C (104°F) 52.2 cSt52.2 cSt
Kinematic Viscosity at 100°C (212°F) 7.7 cSt7.7 cSt
ASTM Color 1.51.5L
 
Descriptive Properties
ChlorinePresent
Fatty OilPresent
PhosphorusPresent
SulfurPresent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Soluble D

WTEXA299 / 77178

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.