MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Protectosil® AQUA-TRETE® BHN PLUS Surface Treatment
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Product Description: A clear penetrating breathable VOC compliant surface treatment for use on concrete, brick masonry, concrete masonry units and natural stone. The unique silane treatment penetrates into the substrate and chemically bonds with silica to form a permanent attachment of the water repellent molecule. In addition, an oil repellent additive resist the ingress of motor oil, transmission fluid, diesel fuel and other automotive fluids. This additive also repels food products such as mustard, ketchup, food grease, milk, wine, beer and soft drinks. Creates a deep hydrophobic layer which prevents the ingress of water and waterborne contaminants from entering the substrate and causing premature deterioration. By combining a low surface tension with a tailored rate of reaction, Protectosil BHN PLUS is able to move through the moisture boundary layer which lines the pore structure of the substrate. This permits the development of uniform gradient permeation or a consistent level of protection throughout the entire depth of penetration. This allows fro a longer life of the treatment especially on wearing surfaces.

Applications: For use on vertical or horizontal concrete and masonry surfaces to repel water and oil based materials from penetrating into the substrate. Reduces staining and discoloration of concrete, brick masonry, limestone, marble, granite, natural stones and other building materials due to oil and water borne contaminates. For use on reinforced concrete to protect against corrosion due to water, deicing salts and salt water. Apply to masonry to prevent the ingress of wind driven rain white maintaining surface appearance and breathability.

Advantages: Protectosil BHN PLUS is a moisture of an alkyltralkoxy silane and a proprietary oil repellent additive. Protectosil BHN PLUS penetrates deeper than traditional silane and siloxane products due to its unique chemistry. This deeper penetration gives a long lasting, high performance water and chloride screen. By greatly reducing water entering the substrate and with it beign a breathable system, as “drying out” of the substrate occurs. The oil repellent additive creates an area of extremely low surface tension on the substrate. This effect renders the surface resistant to the ingress of oil based materials. In addition, the repellent effect against food product is much greater than that imparted by traditional water repellent. The primary function of the Protectosil BHN PLUS is to allow easier cleanup and reduce staining of the substrate due to the absorption of various oil and water based contaminants. If spills are not cleaned up in a timely manner staining and absorption into the substrate will still occur. The main benefits of the product are:

  • Excellent resistance to automotive fluids
  • Excellent repellency of food products
  • Reduces staining
  • Excellent resistance to chloride ion ingress
  • Breathable system
  • Mitigation of AAR & ASR deterioration
  • Deep penetration into substrate
  • No change in surface appearance
  • High resistance to alkali attack
  • Long service life

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.887 g/cc
Volatile Organic Compounds (VOC) Content 400 g/l
 
Thermal PropertiesOriginal ValueComments
Flash Point 28.9 °C
 
Descriptive Properties
Colorwater white
Content94%active

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIM125 / 197329

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.