MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

P & P Technology MS-N Nickel Graphite Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: P & P Technology conductive nickel/graphite adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exposed to atmospheric moisture.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.29 g/cc2.29 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565
Elongation at Break 210 %210 %
Tear Strength 90.0 kN/m514 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.060 ohm-cm0.060 ohm-cm
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 600 g/min600 g/min
Cure Time 15.0 min0.250 hourSkin over time
 720 - 1440 min12.0 - 24.0 hourFull cure for handling
Tack-Free Time 90.0 min1.50 hour
 
Descriptive Properties
ColorDark Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPPTEC019 / 133483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.