MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Esstech V-115-1104 Aluminosilicate Glass-Ceramic
Categories: Ceramic; Glass; Glass Ceramic; Oxide; Silicon Oxide

Material Notes: The refractive index of aluminosilicate glass filler matches that of bisGMA and is very close to our X-970-0000. It has a negative coefficient of thermal expansion, which means it contracts slightly upon heating. This glass contains no barium and therefore has no x-ray opacity making it ideal to blend with our other glass fillers. CAS # 65997-17-3.

Information provided by ESSTECH, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.50 g/cc
Particle Size 10.4 µmmedian
 
Thermal PropertiesOriginal ValueComments
CTE, linear -2.30 µm/m-°C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.54
 
Component Elements PropertiesOriginal ValueComments
Al2O3 20 %
SiO2 71 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott Glass 8240 Alkaline Earth Aluminosilicate Glass
Corning 1724 Aluminosilicate Crushed/Powdered Glass
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Schott NEO 1730 Alkaline Earth Aluminosilicate Glass
712-3 Nextrema® Tinted Glass Ceramic/SCHOTT

PESST001 / 108272

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.