MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Polypropylene AUTOMOTIVE PPC 3060 MW5 is a heterophasic copolymer with a Melt Flow index of 7 g/10 min.

Polypropylene AUTOMOTIVE PPC 3060 MW5 is a high impact copolymer with heat stabilization package.

Polypropylene AUTOMOTIVE PPC 3060 MW5 has been especially developed for use in automotive applications.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccISO 1183
Bulk Density 0.525 g/ccISO 1183
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ISO 868
Tensile Strength, Yield 25.0 MPaISO 527-2
Elongation at Yield 6.0 %ISO 527-2
Tensile Modulus 1300 MPaISO 527-2
Flexural Modulus 1200 MPaISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²
@Temperature -20.0 °C
ISO 180
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -20.0 °C
ISO 179
 13.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C120°C per hour; ISO 752
Vicat Softening Point 65.0 °C
@Load 5.10 kg
50°C per hour; ISO 306
 135 °C
@Load 1.02 kg
50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 3120 MU5 Polypropylene, Heterophasic Copolymer, Automotive
Total PPC 3150 MX5 Polypropylene, Heterophasic Copolymer, Automotive
Overview of materials for Polypropylene Copolymer

PTOTAL848 / 130573

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.