Borcycle MD4481SY is a virgin/recycled PP solution compound with 40% post-consumer recycled and 40% mineral filler. Products originating from this grade have an excellent balance between stiffness and impact strength also at elevated temperature. The product is available in black color. Typical characteristics: Borcycle" MD4481SY can be described with following typical characteristics: - High heat stabilized
- Good flow behavior
- Good stiffness and impact strength balance
Applications: - Appliances
- White goods
- Injection-molded non-food applications
- Structural parts
- Small appliances
To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.Information provided by Borealis AG |