MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound NX11302 Polycarbonate + ABS (PC+ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: LNP THERMOCOMP NX11302 compound is based on Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend containing proprietary fillers. Added features of this grade include: Colorable, Improved Plating Surface and Mechanical Performance suitable for Laser Direct Structuring (LDS) applications.

Features: Laser Direct Structuring,Circuit Solution,Colorable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
Water Absorption 0.010 %
@Time 86400 sec
0.010 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0100 %0.0100 %23°C/50% RH/24 hrs; ASTM D570
 0.0100 %0.0100 %Injection Molding
Viscosity 14 cP
@Load 5.00 kg,
Temperature 260 °C
14 cP
@Load 11.0 lb,
Temperature 500 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.0 MPa6670 psi50 mm/min; ASTM D638
Tensile Strength, Yield 47.0 MPa6820 psi50 mm/min; ASTM D638
Elongation at Break 75 %75 %50 mm/min; ASTM D638
Elongation at Yield 4.6 %4.6 %50 mm/min; ASTM D638
Tensile Modulus 2.35 GPa341 ksi50 mm/min; ASTM D638
Flexural Strength 78.0 MPa11300 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 79.0 MPa11500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.23 GPa323 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 550 J406 ft-lbASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.94
@Frequency 1e+9 Hz
2.94
@Frequency 1e+9 Hz
IEC 60250
Dissipation Factor 0.0057
@Frequency 1e+9 Hz
0.0057
@Frequency 1e+9 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 71.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
39.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
@Thickness 3.20 mm
223 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94 HB
@Thickness >=0.600 mm
HB
@Thickness >=0.0236 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 220 - 260 °C428 - 500 °F
Zone 2 215 - 255 °C419 - 491 °F
Zone 3 215 - 255 °C419 - 491 °F
Melt Temperature 220 - 260 °C428 - 500 °FInjection Molding
Mold Temperature 40.0 - 75.0 °C104 - 167 °F
Drying Temperature 85.0 - 95.0 °C185 - 203 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.500 - 0.900 MPa72.5 - 131 psi
Shot Size 50 - 70 %50 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 50 - 100 rpm50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81745 / 289692

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.