MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® 864 Polyester Packaging Film, 48 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

Melinex® 864 is a polyester film, chemically treated on two sides. Both sides are designed for printing and extruded polyethylene adhesion. One side is enhanced to promote metal adhesion. Melinex® 864 currently is approved for indirect food contact applications. Melinex® 864 is biaxially oriented, two side treated, polyester film which is compliant with Food and Drug Administration food additive regulation 21CFR 177.1630. It can be used in applications requiring direct food contact with all types of food (excluding alcoholic beverages) at temperatures up to and above 250°F (including oven baking or cooking) and for alcoholic beverages (not to exceed 50% alcohol by volume) at ambient temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/cc
Moisture Vapor Transmission 0.660 cc-mm/m²-24hr-atmTested per ASTM F372 at 100°F, 90% RH.
Oxygen Transmission 1.42 cc-mm/m²-24hr-atmTested per ASTM D1434 at 77°F, 75% RH.
Thickness 0.480 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 110 %ASTM D882A
Film Elongation at Break, TD 80 %ASTM D882A
Coefficient of Friction, Dynamic 0.40ASTM D1894
Coefficient of Friction, Static 0.50ASTM D1894
Film Tensile Strength at Break, MD 214 MPaASTM D882A
Film Tensile Strength at Break, TD 238 MPaASTM D882A
 
Optical PropertiesOriginal ValueComments
Haze 3.5 %Gardner; ASTM D1003
Transmission, Visible 90 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® 822 Polyester Packaging Film, 48 Gauge
DuPont Teijin Films Mylar® OB01 Polyester Packaging Film, 50 Gauge
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 50 Gauge
Borealis Borseal™ TD110BF Terpolymer for BOPP Film
DuPont Teijin Films Mylar® 854 Polyester Packaging Film, 60 Gauge

PDU7A9 / 33199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.