A Linear low density polyethylene resin produced using advanced gas phase PE process and is intended for use in general purpose injection molding applications. This resin has been designed to have excellent impact strength, rigidity, environmental stress crack resistance and processability. Main characteristics: injection molding, general purpose applications, excellent low temperature impact strength, rigidity, stress crack resistance and processability, very narrow molecular weight distribution. Processing Notes: Plaque molded and tested in accordance with ASTM D4976 Information provided by ETHYDCO. |