MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Synfoam® AI-42 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Pre-cast. SynFoam AI provides a combination of excellent strength and high temperature property retention along with outstanding acoustic properties. SynFoam AI was developed for use in Naval applications conforming to drawing numbers 5819079 and 5856846. SynFoam AI has been used to provide acoustic insulation for prime contractors within the US department of defense. SynFoam AI is available as precast sheets that can be machined to user specifications up to a maximum size of 2" x 12" x 24". SynFoam AI is easily machined into small shapes and can be bonded together if larger structures are required. Custom formulation services utilizing the AI matrix are available and we also provide final machining services.

Information provided by Synfoam®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 40.0 - 44.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 5350 psi
Compressive Strength 12000 psi
Compressive Modulus 300000 psi
Shear Strength 5000 psi
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 140 °C
 
Descriptive Properties
Depth Rating (m)9750
Sound Velocity (m/s)2800

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg AEM Eccofloat® TG-24/2000 Syntactic Foam
Matrix 999225 Composite Syntactic Foam
Engineered Syntactic Systems MZ-32 Deep Water Syntactic Foam
Coastal Enterprises Plus™ PBHT-48 High Density Urethane Foam

PSYNF001 / 192876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.