Application: Special monomer for thermosetting paints and self-crosslinking emulsions. Appearance: Colorless, solid, crystalline Odor: None CAS: 79-39-0 Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale. |