MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® D1155 J (SBS) Liner Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1155 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Japan in the physical form(s) outlined in the grade nomenclature:
D1155 JOP - supplied as dusted dense pellets
D1155 JO - supplied as dusted crumb

Region: North America, Europe, Asia Pacific, Japan, and South America

Uses: Kraton D1155 J Polymer is used as a modifier of polymers and in formulating adhesives, sealants and coatings. It is also used in compounds for technical and footwear applications.

Applications: Compounding and Personal Hygiene

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/cc
Volatiles <= 0.20 %
@Temperature 110 °C,
Time 7200 sec
JOP
 <= 1.0 %
@Temperature 110 °C,
Time 7200 sec
JO
Melt Flow 1.8 - 4.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Ash <= 0.20 %JOP; ISO 247
 <= 1.0 %JO; ISO 247
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87
@Time 30.0 sec
ISO 7619
Tensile Strength 28.0 MPaISO 37
Elongation at Break 800 %ISO 37
300% Modulus 0.00290 GPa
@Strain 300 %
ISO 37
 
Descriptive Properties
ContentBound Styrene40 percent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1184 A (SBS) Branched Block Copolymer
INEOS Styrolution K-Resin® KR03 Styrene Butadiene Copolymer (SBC)
INEOS Styrolution K-Resin® KR01 Styrene Butadiene Copolymer (SBC)
A. Schulman Diamond SBS 1031 Clear Styrene Butadiene Copolymer
Kraton® D1118 K (SBS) Diblock Copolymer

PKRA9826 / 132725

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.