System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
KEP Kepital® FG2025K Acetal Copolymer, 10% Glass Fiber
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Copolymer, 10% Glass Fiber Reinforced
Material Notes:
10% glass fiber filled medium viscosity grade good for general injection molding. FG2025K is good for parts requiring moderate stiffness, strength, creep resistance, and HDT.
Information provided by KEP Americas.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.47
g/cc
ISO 1183
Water Absorption
0.20 %
ISO 62
Melt Flow
13
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength
110
MPa
50 mm/min; ISO 527
Elongation at Break
3.8 %
50 mm/min; ISO 527
Flexural Strength
160
MPa
ISO 178
Flexural Modulus
4750
MPa
ISO 178
Charpy Impact, Notched
6.50
kJ/m²
ISO 179
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+16
ohm-cm
IEC 60093
Surface Resistance
1.00e+16
ohm
IEC 60093
Thermal Properties
Original Value
Comments
CTE, linear
80.0
µm/m-°C
ISO 11359
Melting Point
165
°C
ISO 3146
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
KEP Kepital® FG2025 25% Glass Fiber Reinforced Acetal Copolymer
Celanese Celcon® GC10 POM, 10% Glass Reinforced
KEP Kepital® F20-03 Acetal Copolymer, Medium viscosity
BASF Ultraform® N2200 G43 POM
Celanese Celcon® M90™ POM, Unfilled
PKEP9900 / 185576
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.