MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Novatex® EP NLGI Grade 1
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Texaco Novatex EP are water resistant, extreme pressure greases. They are manufactured using highly refined, select high viscosity index base oils, a calcium soap, and a specifically selected additive package containing extreme pressure additives as well as corrosion and rust inhibitors.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 222904; MSDS Number: 9007

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 62Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 1104 SUSSee Note 3.
Saybolt Viscosity at 210°F 80 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 206 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 15 cStSee Note 3.
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 46
Four Ball Extreme Pressure, Weld Load 250 kg
Four Ball Wear 0.400 mmScar Diameter
Penetration P(60), 1/10 mm 325Unknown Amount of Work, 25°C (77°F)
Timken Test 40.0 lbOK Load
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °CSee Note 2.
Minimum Service Temperature, Air -29.0 °CSee Note 1.
Flash Point 162 °CSee Note 3.
Dropping Point 260 °C
 
Descriptive Properties
ColorBrown
Corrosion, Copper Strip1B
TextureSmooth
Thickener, %7Calcium
Water Washout, wt%2Loss at 175°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Marfak® 0
ChevronTexaco Marfak® Heavy Duty 2
ChevronTexaco Novatex® EP NLGI Grade 000
ChevronTexaco Thuban® SAE 250
ChevronTexaco Thuban® SAE 80W-90

WTEXA261 / 77140

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.