MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® OL13AT Polyester Packaging Film, 100 Gauge  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

Mylar® OL13AT is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and frozen foods. Mylar® OL13AT is dual ovenable film which provides very strong, aggressive seals to polar substrates such as amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, and polyvinylchloride (PVC). Mylar® OL13AT does not seal to polyethylene, polypropylene, or polystyrene. DuPont Teijin Films offers another family of lidding films (RL types) for sealing to these substrates. Mylar® OL13AT is similar to OL12AT but has a thicker seal layer than Mylar® OL12AT to give enhanced seal strength. In general, Mylar® OL13AT can produce non-peeling, near "lock-up" type seals and is recommended for hot fill applications where non-peeling seals are desired. It can also be used in some "post-pasteurized" (steam sterilization) applications where the pressure balance in the package can be properly controlled (via vacuum or overpressure). Mylar® OL13 lidding films have excellent grease and oil resistance.

Mylar® OL13AT lidding films are available with anti-fogging capability to provide better clarity when stored and displayed in refrigerated conditions. This film type is marketed by DuPont Teijin Films as OL13AT and is available with corona treatment on opposite side of film from the heat seal layer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Calculated from nominal thickness and yield
Moisture Vapor Transmission 0.610 cc-mm/m²-24hr-atm1.55 cc-mil/100 in²-24hr-atmProc. E; ASTM E96
Oxygen Transmission 2.36 cc-mm/m²-24hr-atm5.99 cc-mil/100 in²-24hr-atmTested per ASTM D3985 at 22°C
Thickness 25.4 microns1.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 110 %110 %ASTM D882
Film Elongation at Break, TD 80 %80 %ASTM D882
Secant Modulus 3.79 GPa550 ksiStiffness Modulus; ASTM D882
Tear Strength Test 1.11.1lb Graves; ASTM D1004
Film Tensile Strength at Break, MD 172 MPa24900 psiASTM D882
Film Tensile Strength at Break, TD 241 MPa35000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU7D8 / 33228

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.