MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Epoxies, Etc 20-2521 Polyurethane Potting & Encapsulating Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Description: 20-2521 is a high performance two component urethane system. This easy to use polyurethane is very low in viscosity and ideal for potting or encapsulating delicate electronic components. 20-2521 exhibits very low shrinkage, stress, and exotherm throughout the cure cycle. This system is also well known for its outstanding thermal shock and excellent dielectric properties. 20-2521 is ideal for potting applications where a wide operating temperature (-55 to +130°C) is required. It is also a good choice when exposure to salt water, mild acids and bases, and aliphatic hydrocarbons is expected.

Features:

  • Does not contain MOCA or TDI
  • Low stress on components
  • Excellent dielectric properties
  • Low viscosity
  • Easy to handle
  • Low shrinkage
  • Very good thermal shock and vibration resistance ??Hydrolytic stability

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccIsocyanate
 1.60 g/cc1.60 g/ccPolyol
Water Absorption  0.19 %
@Time 86400 sec
0.19 %
@Time 24.0 hour
 0.55 %
@Time 605000 sec
0.55 %
@Time 168 hour
Viscosity 200 cP200 cPIsocyanate
 5500 cP5500 cPMixed
 15000 cP15000 cPPolyol
Storage Temperature 21.0 - 29.0 °C69.8 - 84.2 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
Tensile Strength 11.0 MPa1600 psi
Elongation at Break 40 %40 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.20e+14 ohm-cm1.20e+14 ohm-cm
Surface Resistance 4.60e+13 ohm4.60e+13 ohm
Dielectric Constant 4.8
@Frequency 100 Hz
4.8
@Frequency 100 Hz
Dielectric Strength 24.8 kV/mm630 kV/in
Dissipation Factor 0.72
@Frequency 60 Hz
0.72
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 160 µm/m-°C88.9 µin/in-°F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Shrinkage 0.71 %0.71 %
 
Processing PropertiesMetricEnglishComments
Cure Time  40.0 min
@Temperature 85.0 °C
0.667 hour
@Temperature 185 °F
 90.0 min
@Temperature 65.0 °C
1.50 hour
@Temperature 149 °F
 150 min
@Temperature 45.0 °C
2.50 hour
@Temperature 113 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 75.0 min75.0 min
 
Descriptive Properties
ColorBlack
Mix Ratio100:20Iso:Polyol, by weight
 100:26Iso:Polyol, by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX019 / 316696

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.