MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow 620I Linear Low Density Polyethylene (LDPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes:
  • For extruded foam applications
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D792
ESCR 100% Igepal® <= 1.0 hour
@Temperature 50.0 °C
F50; Compression molded; ASTM D1693
Melt Index of Compound 1.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 46Compression molded; ASTM D2240
Tensile Strength at Break 1500 psiCompression molded; ASTM D638
Tensile Strength, Yield 1500 psiCompression molded; ASTM D638
Elongation at Break 470 %Compression molded; ASTM D638
Elongation at Yield 3.0 %Compression molded; ASTM D638
Flexural Modulus 40000 psiCompression molded; ASTM D790 B
Tensile Impact Strength 70.0 ft-lb/in²Compression molded; ASTM D1822, Type S
 
Thermal PropertiesOriginal ValueComments
Melting Point 235 °FDow Method (DSC)
Crystallization Temperature 100 °CDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 104 °FCompression molded; ASTM D648
Vicat Softening Point 210 °FASTM D1525
Brittleness Temperature <= -105 °FCompression molded; ASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont 20 Series 20-6064 Specialty Polyethylene Resin
Dow 611A Low Density Polyethylene (LDPE)
Dow 4012 Low Density Polyethylene (LDPE)
Dow 4010 Low Density Polyethylene (LDPE)
Dow 608A Low Density Polyethylene (LDPE)

PDOW1239 / 30457

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.