MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Lupranate® 274 Isocyanate
Categories: Fluid

Material Notes: Description: Lupranate® 274 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Lupranate 274 Isocyanate is suitable for the production of rigid insulation foams by molding, spraying, and frothing. It is also used for rigid and semi-flexible integral skin foams, adhesives, sealants, elastomers, and high-resiliency flexible foams. In low catalyzed rigid urethane formulations, the foam rise time can be lengthened by 20-30%. The slower reactivity can be advantageous in applications such as large rigid foam panels or molded flexible foams.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Viscosity 200 cP200 cP
Vapor Pressure 2.67e-7 bar
@Temperature 25.0 °C
0.000200 torr
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Boiling Point >= 190 °C
@Pressure 0.000667 MPa
>= 374 °F
@Pressure 0.0967 psi
Flash Point 200 °C392 °F
 
Descriptive Properties
ColorDark Brown
CompositionHydrolyzable Chlorine0.00035
 NCO content0.315

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Lupranate® 219 Isocyanate Modified MDI
BASF Lupranate® 259 Isocyanate
BASF Lupranate® 253 Isocyanate
BASF Lupranate® 245 Isocyanate
BASF Lupranate® 227 Isocyanate

PBASG0661 / 132294

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.