Reinforced, flame retardant PA66 offers high mechanical properties, good heat resistance, good dimensional stability, good flammability, good processability. Reinforced, reinforced flame retardant PA66 is used for automotive parts, furniture parts, electric tool, transformer skeleton, thin-walled relay, electric device parts, residual current operated protective devices, electrical appliances parts, vidicon parts, etc.Information provided by Yuyao Zhongfa Engineering Plastics CO., LTD |