MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro HYPERLITE® E-824 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Hyperlite E-824 is a 5,000-molecular-weight polyoxyalkylene polyol, which is used in a broad range of urethane foam and other applications.

Properties / Applications: Hyperlite E-824 is a 5,000-molecular weight polyoxyalkylene polyol, which is used in a broad range of urethane foam and other applications. This polyol is an ethylene oxide adduct of a polyoxypropylene triol. Because it contains a high percentage of primary hydroxyl groups, it has a relatively high rate of reactivity. It is compatible with most polyether polyols and can be blended with other diols, triols, and polymer polyols to achieve desirable modifications of product properties. Hyperlite E-824 polyol is especially suited for low-density rapid-demold high-resiliency (HR) foam. It is typically used in molded urethane seating applications. As with any product, the use of Hyperlite E-824 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/cc
Bulk Density 64.6 lb/ft³
 
Thermal PropertiesOriginal ValueComments
Flash Point 166 °CPMCC
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmodur® XP 2619 Polyurethane
Covestro DESMODURE® N 100A Polyurethane
Covestro DESMODURE® N 3200A Polyurethane
Covestro DESMODURE® N 3300A Polyurethane
Covestro DESMODURE® N 3368A BA/SN Polyurethane

PCOVEST0789 / 202572

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.