MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kazanorgsintez 273-83 High Density Polyethylene Composite
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Production Method: Gaseous-phase method.

Application: Composition of HD grade 273-83 is intended to obtain by method of extrusion products of industrial, cultural, and general use as well as goods contacting with food.

Information Provided by Kazanorgsintez

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 - 0.955 g/cc
Volatiles <= 0.090 %Superior Class
 <= 0.10 %1st Class
Melt Flow 0.40 - 0.65 g/10 min±10% Superior Class, ±18% 1st Class
Ash <= 0.040 %Superior Class
 <= 0.060 %1st Class
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 22.6 MPaSuperior Class, 1st Class
Elongation at Break >= 450 %1st Class
 >= 700 %Superior Class
Tear Strength Test >= 21.6MPa, 1st Class
 >= 29.4MPa, Superior Class
 
Descriptive Properties
Amount of impurities [pcs]201st Class
 5Superior Class

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NIZHNEKAMSKNEFTEKHIM PE 6252J (526F2) High Density Polyethylene

PKAZAN013 / 127332

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.