MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Magnesium HM31A-T5, Extruded Solid Shapes
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes:

Key Words: UNS M13312; Mg
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.81 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 300 MPa
Tensile Strength, Yield 270 MPa
Elongation at Break 10 %in 50 mm
Tensile Modulus 45.0 GPa
Compressive Yield Strength 170 MPa
Ultimate Bearing Strength 470 MPa
Bearing Yield Strength 330 MPa
Poissons Ratio 0.35
Shear Modulus 17.0 GPa
Shear Strength 185 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000570 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 331 J/g
CTE, linear 26.0 µm/m-°C
@Temperature 0.000 - 100 °C
 28.0 µm/m-°C
@Temperature 25.0 - 260 °C
Estimated from similar Mg alloys
Specific Heat Capacity 1.00 J/g-°C
Thermal Conductivity 104 W/m-K
Melting Point >= 482 °CIncipient Melting
Solidus 605 °C
Liquidus 650 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 370 - 540 °CHot Working
Recrystallization Temperature 455 °C
 
Component Elements PropertiesOriginal ValueComments
Magnesium, Mg 96 %As Remainder
Manganese, Mn >= 1.2 %
Thorium, Th 2.5 - 3.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium EA55RS-T4, Extruded
Magnesium AZ61A-F, Extruded Solid Shapes
Magnesium AZ80A-T5, Extruded
Magnesium EA65RS-T4, Extruded
SAE SiC/AZ91 Magnesium Matrix Composite, as cast

MMHM32 / 12448

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.