MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type 450 Stainless Steel, 25 mm diameter bar, solution annealed
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S40000 Series Stainless Steel

Material Notes: Martensitic, age-hardenable, very good corrosion resistance with moderate strength, resists atmospheric corrosion including salt water atmospheres, excellent resistance to rusting and pitting in 5 and 20% salt spray at 35°C and oxidation up to 650°C, maximum service temperature for continuous service is 425°C. Niobium content minimum is 8 times the carbon content.

Key Words: UNS S45000, AMS 5763, ASME SA564 (XM-25), T S45000, ASME SA 705 (XM-25), ASTM A564 (XM-25), ASTM A693 (XM-25), ASTM A705 (XM-25)
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 278Converted from Rockwell C hardness.
Hardness, Knoop 296Converted from Rockwell C hardness.
Hardness, Rockwell C 28
Hardness, Vickers 287Converted from Rockwell C hardness.
Tensile Strength, Ultimate 986 MPa
Tensile Strength, Yield 814 MPa
@Strain 0.2 %
Elongation at Break 13.3 %Gage length 1 in. (25 mm)
Modulus of Elasticity 204 - 215 GPa
Notched Tensile Strength 1525 MPa
Bulk Modulus 166 GPa
Poissons Ratio 0.283
Shear Modulus 83.9 GPa
Charpy Impact 125 - 141 J
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.1 µm/m-°C
@Temperature 20.0 - 100 °C
 10.4 µm/m-°C
@Temperature 24.0 - 260 °C
 10.6 µm/m-°C
@Temperature 24.0 - 315 °C
annealed at 1040°C, water quenched
 10.8 µm/m-°C
@Temperature 24.0 - 370 °C
annealed at 1040°C, water quenched
 11.0 µm/m-°C
@Temperature 24.0 - 425 °C
annealed at 1040°C, water quenched
 11.1 µm/m-°C
@Temperature 24.0 - 480 °C
annealed at 1040°C, water quenched
 11.2 µm/m-°C
@Temperature 24.0 - 595 °C
annealed at 1040°C, water quenched
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 20.7 W/m-KTypical value for stainless steel.
Maximum Service Temperature, Air 425 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.050 %
Chromium, Cr 15 %
Copper, Cu 1.5 %
Iron, Fe 74 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo 0.75 %
Nickel, Ni 6.0 %
Niobium, Nb (Columbium, Cb) >= 0.40 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 13 mm (0.5 in.) round
AISI Type 450 Stainless Steel, 25 mm diameter bar, aged at 455°C (850°F)
AISI Type S45500 Stainless Steel, annealed at 815°C (1500°F) for 30 minutes, water quenched, bar
Kinetics MIM 17-4PH Stainless Steel (H900 Condition)
304 Stainless Steel

MQM450A / 13809

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.