Master Bond MasterSil 700 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. It remains flexible and provides excellent service over the broad temperature range of -75°F (-60°C) to +400°F (205°C). |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |