MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Socomore Aeroglaze® A276 Reflective Polyurethane
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: Aeroglaze® A276 reflective polyurethane gives a hard, flexible, colorfast, non-chalking surface that is resistant to most acids, alkaline detergents, lubricants, and chemicals.

Socomore acquired the Aeroglaze® and Chemglaze® product lines from Lord in September 2016.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D1475-85
Solids Content 40.6 %by volume; ASTM D2369-87 Modified
 56 %by weight; ASTM D2369-87 Modified
Volatile Organic Compounds (VOC) Content 520 g/lASTM D3960-87
Brookfield Viscosity 250 cP
@Temperature 25.0 °C
ASTM D2196-66; LVT
Outgassing - Total Mass Loss 0.99 %ASTM E595-77
 
Mechanical PropertiesOriginal ValueComments
Gardner Impact 160 in-lbDirect
 160 in-lbReverse
 
Thermal PropertiesOriginal ValueComments
Flash Point 19.3 °CSetaflash, Closed Cup; ASTM D3278-82
 
Optical PropertiesOriginal ValueComments
Gloss 93 %60°
Emissivity (0-1) 0.90Normal; ASTM E-595-77
 
Processing PropertiesOriginal ValueComments
Cure Time 336 hour
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceGloss White
Conical Mandrel BendPasses 1/8"ASTM D522
Solar Absorption0.23Gier-Dunkle Integrating Sphere
Theoretical Coverage (ft²/gallon/mil)650

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Ceramics MICROSIL Microporous Insulation
Solvay Thornel® VCL Carbon Fiber Cloth
Solvay Thornel® VCK Carbon Fiber Cloth
Solvay Thornel® VCK Carbon Cloth Laminate with Mil R-9299 Resin
Socomore Aeroglaze® Z306 Absorptive Polyurethane

PLORD125 / 86133

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.