BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or extruded in pre -weighted slugs. Typical applications are outdoor lighting fixtures and grill shelves. |