MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vyncolit X689 Novolac Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Glass fiber filled and molybdeendisulfide modified phenolic molding compound with excellent mechanical and thermal properties and lower thermal expansion coefficient. It has excellent friction properties.

USES: Water pump seals and self-lubricating bearings.

Information provided by Vyncolit, a Sumitomo Bakelite Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 g/ccPowder Density; ISO 60
Density 1.70 g/ccRelative Density; ISO 1183
Linear Mold Shrinkage 0.0050 cm/cmInjection Molding; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPaISO 527
Elongation at Break 0.70 %Tensile; ISO 527
Tensile Modulus 15.0 GPaISO 527
Flexural Strength 160 MPaAt Rupture; ISO 178
Flexural Modulus 12.0 GPaISO 178
Flexural Strain at Break 1.5 %ISO 178
Compressive Strength 245 MPaISO 604
Charpy Impact Unnotched 1.00 J/cm²ISO 179
Charpy Impact, Notched 0.300 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 30.0 kV/mmIEC 243
Comparative Tracking Index 125 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 20.0 °C
TMA
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature 20.0 °C
TMA
Deflection Temperature at 1.8 MPa (264 psi) 180 °CISO 75 Af
Shrinkage 0.15 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
ISO typePF 2 C1
Main FillerGlass Fiber & Molybdenum Disulfide
Molding MethodCompression, transfer, injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vyncolit X681 Novolac Phenolic
Raschig Group DECAL® 937 Phenolic
Raschig Group DECAL® 152CL Phenolic
Plenco 5118 Phenolic, Granular, Compression Molded
Plenco 4300 Phenolic, Granular, Compression Molded

PVYNC006 / 72214

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.