Dry as molded. Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long product life to gears, bearings, cams, fasteners, and other load bearing parts. Nylene 451 chemically resists oil
and grease.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |