MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 24955N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24955N is a general purpose thermoplastic vulcanizate used in automotive and industrial applications. This grade is a medium hardness, low density, lubricated grade that can be processed by injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Light Stabilized; Low Density; Low Specific Gravity; Lubricated; Medium Flow; Medium Hardness; Slip

Uses: Expansion Joint; Gaskets; Glazing; Grommets; Plugs; Shock Absorbing Pads; Tubing; Weatherstripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccISO 1183
Viscosity 161 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Apparent; ASTM D3835
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 54
@Time 15.0 sec
Injection Molded; ISO 868
 55
@Time 5.00 sec
Injection Molded; ISO 868
 57
@Time 1.00 sec
Injection Molded; ISO 868
 53.7
@Treatment Temp. 125 °C,
Time 15.0 sec
Injection Molded, Change in Air, 168; ISO 888
 55.7
@Treatment Temp. 125 °C,
Time 5.00 sec
Injection Molded, Change in Air, 168; ISO 888
 57.1
@Treatment Temp. 110 °C,
Time 15.0 sec
Injection Molded, Change in Air, 1008; ISO 888
 57.9
@Treatment Temp. 125 °C,
Time 1.00 sec
Injection Molded, Change in Air, 168; ISO 888
 58.8
@Treatment Temp. 110 °C,
Time 5.00 sec
Injection Molded, Change in Air, 1008; ISO 888
 61
@Treatment Temp. 110 °C,
Time 1.00 sec
Injection Molded, Change in Air, 1008; ISO 888
Tensile Strength at Break 450 psiAcross Flow, Type 1, 20 in/min; ISO 37
 479 psiFlow, Type 1, 20 in/min; ISO 37
 421 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 464 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
 465 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 479 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 254 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 383 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 276 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air in 1008 hr; ISO 188
 282 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air in 168 hr; ISO 188
 414 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air in 1008 hr; ISO 188
 425 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air in 168 hr; ISO 188
Elongation at Break 180 %Flow, Type 1, 20 in/min; ISO 37
 250 %Across Flow, Type 1, 20 in/min; ISO 37
 139 %
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 146 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 210 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 236 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 75.0 pliMethod Ba, Angle (Unnicked), Flow, 20 in/min; ISO 34-1
 79.0 pliMethod Ba, Angle (Unnicked), Across Flow, 20 in/min; ISO 34-1
Compression Set 15 %
@Temperature 22.8 °C,
Time 79200 sec
Type A; ISO 815
 24 %
@Temperature 70.0 °C,
Time 79200 sec
Type A; ISO 815
 28 %
@Temperature 90.0 °C,
Time 252000 sec
Type A; ISO 815
 41 %
@Temperature 125 °C,
Time 252000 sec
Type A; ISO 815
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -76.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 374 - 446 °FInjection, Melt
Rear Barrel Temperature 344 - 416 °FInjection
Middle Barrel Temperature 354 - 426 °FInjection
Front Barrel Temperature 364 - 436 °FInjection
Nozzle Temperature 374 - 446 °FInjection
Zone 1 330 - 400 °FExtrusion
Zone 2 340 - 410 °FExtrusion
Zone 3 350 - 420 °FExtrusion
Zone 4 355 - 425 °FExtrusion
Zone 5 360 - 430 °FExtrusion
Die Temperature 374 - 440 °FExtrusion
Mold Temperature 95.0 - 140 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 125 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 120 rpmInjection
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1200 / 237691

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.